Bowing Brick Walls in Perth

Eric MorrisonBuilding Inspections

Bowing Brick Walls Perth: Causes and Structural Warning Signs

Bowing brick walls Perth showing corroded wall ties, horizontal cracking and outward masonry movement

Illustration showing how deteriorated wall ties can contribute to outward bowing and cracking in double-brick walls.

Bowing brick walls in Perth homes can indicate structural movement, deteriorating wall ties or inadequate masonry support. Although some movement develops gradually, significant bowing should never be ignored.

Double-brick construction is common throughout Perth, particularly in older properties. Over time, moisture exposure, foundation movement and deterioration of structural connections can affect the stability of brick walls.

However, a bowed or bulging wall does not automatically indicate a major structural defect. The extent of movement, wall construction and surrounding conditions must be considered.

At Master Building Inspectors, our registered WA builders assess structural cracking and masonry movement during building inspections throughout Perth.

Why Brick Walls Bow in Perth

Several factors can contribute to bowing brickwork. In some properties, more than one issue may be present.

Corroded Wall Ties

Wall ties connect the inner and outer leaves of cavity brickwork. They provide lateral restraint and help the two walls act together.

Older properties may contain galvanised steel ties that have deteriorated through prolonged moisture exposure.

As corrosion develops, the steel can lose strength and its connection to the mortar may weaken. Expanding corrosion products can also cause horizontal cracking within mortar joints.

Where sufficient restraint is lost, sections of brickwork may move outward or become unstable.

However, wall-tie corrosion cannot be confirmed simply because a wall appears bowed. Further investigation may be necessary.

Moisture and Coastal Exposure

Perth’s coastal environment can contribute to the deterioration of masonry components.

Wind-driven rain, salt exposure and prolonged dampness may accelerate corrosion of embedded steel connections.

Other contributing factors include:

  • Blocked or obstructed weep holes.
  • Leaking gutters and downpipes.
  • Raised garden beds against external walls.
  • Paving positioned above damp-proof courses.
  • Poor drainage around the building.

These conditions can increase moisture exposure and contribute to long-term deterioration.

Cracked brick pier identified during a structural inspection in Perth

Foundation Movement

Movement beneath a brick wall can also cause cracking, leaning or distortion.

Perth properties are constructed on varying ground conditions, including sandy soils and areas containing reactive clay.

Potential contributing factors include poor drainage, leaking underground pipes, tree roots and differential footing settlement.

Where movement occurs unevenly, cracking may develop around openings or along mortar joints.

Inadequate Structural Restraint

Brick walls rely on appropriate connections and support to remain structurally stable.

Inadequate wall ties, poorly restrained masonry or previous alterations can reduce structural performance.

Renovations may also affect load-bearing walls and the roof framing they support.

For further information, see our article on Roof Sagging Perth, which explains common structural support defects in existing homes.

Warning Signs of Bowing Brickwork

Visible defects can provide important information about the condition of a masonry wall.

Common warning signs include:

  • Horizontal cracking along mortar bed joints.
  • Stepped cracking through brickwork.
  • Visible outward bulging or leaning.
  • Separation between adjoining walls.
  • Cracking around windows and door openings.
  • Deteriorating or displaced mortar.
  • Doors or windows becoming difficult to operate.
  • Localised brickwork displacement.

These symptoms should be assessed together rather than individually.

Horizontal and Stepped Cracking

Horizontal cracking may be associated with corrosion of embedded steel, structural loading or other movement.

Stepped cracking can occur where differential settlement causes movement through mortar joints.

However, cracking patterns alone cannot establish the underlying cause.

The location, width and extent of cracking are important considerations during an inspection.

Outward Wall Movement

A bowed wall may appear curved when viewed along its length.

In some cases, the middle section moves outward while the upper and lower sections remain relatively straight.

Other walls may lean more uniformly.

Noticeable displacement, particularly where movement appears progressive, warrants further assessment.

Deteriorating Mortar

Mortar deterioration can reduce the integrity of brickwork.

Weathering, moisture exposure and ageing may cause joints to become recessed, powdery or weakened.

Although repointing can address some maintenance defects, it does not necessarily resolve structural movement.

The underlying cause should be established before substantial repairs commence.

Cracking to limestone Perth wall.

Minor Cracking or Structural Movement?

Not every crack indicates a significant structural defect.

Hairline cracking may result from normal building movement, thermal expansion or minor settlement.

However, cracking accompanied by visible distortion deserves closer attention.

Warning signs include:

  • Cracks increasing in width.
  • Significant displacement between adjoining bricks.
  • Cracking extending through masonry units.
  • Wall movement affecting doors or windows.
  • Separation between structural elements.
  • Recent or progressive outward wall movement.

A crack that has remained stable for many years may have different implications from one that is actively widening.

Our article on Structural Problems Found During a Building Inspection explains how structural defects are assessed and why their severity can vary.

Where a wall shows substantial movement or appears unstable, prompt assessment by a structural engineer may be necessary.

Does Bowing Mean Wall-Tie Failure?

No. Bowing brickwork does not automatically confirm corroded or failed wall ties.

Other potential causes include:

  • Differential footing settlement.
  • Inadequate lateral restraint.
  • Poor construction or previous alterations.
  • Thermal or moisture-related movement.
  • Excessive structural loading.
  • Deterioration of supporting components.

Likewise, wall ties may have deteriorated without producing obvious external bowing.

Consequently, an inspection should consider the overall building structure rather than relying on a single visible symptom.

Australian Standards and WA Guidance

Australian Standard AS 3700, Masonry Structures, provides requirements relating to masonry design and construction, including wall ties and structural restraint.

The applicable requirements depend on the building’s age, design and construction circumstances.

The Western Australian Government has also published guidance titled Mitigating Risks and Ensuring the Safety of Pre-1990s Brick Buildings.

This guidance identifies several concerns affecting older masonry buildings, including deteriorating wall ties and inadequate restraint.

It also emphasises the importance of appropriate inspection, maintenance and specialist assessment.

How Building Inspectors Assess Bowing Walls

A structural building inspection involves assessing visible and reasonably accessible building components.

Depending on the circumstances, the inspector may examine:

  • The extent and location of wall displacement.
  • Crack widths and patterns.
  • Brickwork alignment and verticality.
  • Mortar and masonry deterioration.
  • Visible structural connections.
  • Drainage and surrounding ground conditions.
  • Other evidence of building movement.

These observations help establish the significance of the visible defects.

However, a standard visual inspection cannot confirm the condition of wall ties concealed within masonry cavities.

Where deterioration is suspected, additional investigation may involve selective exposure of ties, specialist testing or structural engineering assessment.

Master Building Inspectors provides structural building inspections in Perth to help property owners and buyers understand visible structural concerns.

For buyers unfamiliar with inspection terminology, our guide on How to Read a Building Inspection Report in Perth explains how major defects, recommendations and inspection limitations are presented.

What to Do About Bowing Brick Walls in Perth

If you notice bowing or cracking within your brickwork, avoid assuming the problem is cosmetic.

Consider the following steps:

  1. Photograph visible cracking and record changes over time.
  2. Check for obvious drainage or moisture problems.
  3. Avoid covering significant cracking with render or patching before assessment.
  4. Arrange an inspection where structural movement is suspected.
  5. Obtain specialist engineering advice where significant instability or progressive movement is identified.

For property buyers, identifying structural concerns before a purchase becomes unconditional can be particularly important.

Where significant movement appears in a recently completed home, the builder should also be notified promptly. Our guide to the New Home Defect Liability Period in WA explains the relevant notification requirements. Where substantial bulging, loose masonry or sudden movement is present, keep clear of the affected area and arrange an urgent structural assessment.

Frequently Asked Questions

What Causes Bowing Brick Walls in Perth?

Common contributing factors include deteriorating wall ties, foundation movement, moisture exposure and inadequate structural restraint. The cause should be determined through appropriate inspection and investigation.

Are Bowing Brick Walls Dangerous?

Some walls remain relatively stable despite minor movement. However, significant or progressive bowing can indicate reduced structural stability. Prompt professional assessment is recommended where substantial displacement is evident.

Can Corroded Wall Ties Be Replaced?

Yes. Depending on the construction and condition of the wall, specialist remedial systems may be available. The appropriate repair method should follow investigation and, where necessary, engineering design.

Should I Buy a House With Bowing Brickwork?

Not necessarily a reason to reject the property. However, the cause, severity and likely repair requirements should be understood before proceeding. A structural inspection can help identify concerns requiring further investigation.

Structural Building Inspections Perth

Bowing brick walls should be assessed in the context of the overall building structure.

Although some movement is relatively minor, other defects may indicate significant deterioration or inadequate structural support.

Master Building Inspectors provides independent structural and pre-purchase building inspections throughout Perth.

Our inspections are conducted by registered WA builders, with detailed photographic reports generally provided within 24 hours.

If you are concerned about bowing brickwork, structural cracking or movement within your property, contact Master Building Inspectors to discuss an appropriate inspection.